Crucibles

Porcelain crubiles are autoclavable and can withstand temperatures to 1150° C. To prevent thermal stress cracks, we strongly recommend a heating/cooling rate not exceeding 200° C per hour.  Porcelain crucibles offer excellent resistance to acids and alkalies except for hydrofluoric acid.

Thermal Shock Resistance - average coefficient of expansion from 20° C to 200° C is 3.56 x 10-5, gradually increasing to 4.69 x 10-5 at 1050°C. Every batch of porcelain is heat tested in our factory.

  • Glaze - No softening occurs up to 1000°C, and it is extremely white.
  • Resistance to Chemical Action - Resistance to acids and alkalies is excellent, except for hydrofluoric acid.